Objective. The student will complete assigned metal straightening, MIG/squeeze-type resistance welding, and bolt-on or structural panel replacement tasks on customer vehicles to the quality level accepted by the shop supervisor.
This lesson, its worked examples and its practice questions has not yet been verified by a certified examiner or master technician in the trade or by a certification or approval body. It is a study draft and may contain errors. Do not use it as instructions for work on a job site or on live equipment. Always follow your instructor, your supervising professional, and current official references and regulations.
VoTechWorks program approval and accreditation are still in progress. Credentials are issued only by the certifying bodies named in each program, after their own exams.
During your externship you move from the classroom to the shop floor, where every repair decision affects a real customer's vehicle. The tasks in this phase — metal straightening, MIG and resistance welding, and structural panel replacement — are the core competencies tested by both the I-CAR ProLevel and ASE B-series credentials. Work carefully, log everything, and ask your journeyman supervisor before you are unsure, not after.
Metal straightening begins with reading the damage. Walk around the panel and identify the high spots (stretched or rolled metal above the body line) and low spots (pushed-in areas). The goal is to move metal back toward its original shape without thinning or work-hardening it beyond recovery.
Hammer-on-dolly is used to raise a low spot: hold the dolly directly behind the low area and strike on top of the dolly contact point. The rebound energy raises the metal. Hammer-off-dolly is used to lower a high spot: position the dolly slightly away from the hammer strike so the surrounding metal is supported while the high point is tapped down. Alternate between techniques as the panel approaches alignment.
Stud welding (drawn arc stud welding) is the preferred method when the back side of a panel is inaccessible. Weld steel studs or pins to the low area, then use a slide hammer or pulling bar to draw the dent out incrementally. Remove studs by twisting with pliers after pulling, then file or grind flush. Wear a welding helmet rated for the arc, leather gloves, and flame-resistant clothing during any arc welding operation.
Log every vehicle by its Repair Order (RO) number, the task you performed, the time you spent, and your supervisor's initials before the end of the shift. An incomplete log entry cannot be verified and will not count toward your evaluation.
Before cutting or drilling anything, look up the OEM body repair manual or the applicable I-CAR repair procedure for the exact year, make, and model. Repair procedures specify factory weld locations, weld types, metal grades (including high-strength steel or advanced high-strength steel), seam sealer locations, and anti-corrosion treatment requirements. Never guess at weld count or location on a structural component.
Bolt-on panels (hoods, doors, fenders) are removed by unbolting at the hinge or mounting points. Capture shim locations and note gap measurements before removal so the new panel can be aligned to the same fit.
Welded structural panels — quarter panel sections, uni-rails (front or rear frame rails on unitized bodies), rocker panels, and similar components — require sectioning or full replacement. The procedure typically follows these stages:
1. Establish the correct vehicle dimensions using a tram gauge or electronic measuring system before any cuts are made. Verify against OEM or industry dimension specifications.
2. Cut at OEM-approved sectioning locations only. Use a cut-off disc on an angle grinder; keep the cut straight and minimize heat.
3. Remove factory spot welds using a spot-weld drill bit or cutter. Count the factory welds and match that count with plug welds on the replacement panel.
4. Fit the new panel, re-measure, and clamp. Dimensions must be within the tolerance stated in the repair procedure before welding begins.
5. Perform plug welds (MIG) or squeeze-type resistance spot welds at the marked locations. Match the weld diameter and spacing to factory specifications.
6. Apply seam sealer per the OEM specification at all seams that were originally sealed. Allow proper cure time before priming.
7. Apply weld-through primer or cavity wax to enclosed sections as specified to restore corrosion protection.
MIG (Metal Inert Gas) plug welding is the shop standard for replacing factory spot welds on steel panels. Use the wire diameter, shielding gas mixture, and voltage/wire-speed settings recommended for the metal thickness you are welding. On high-strength steel (HSS) or advanced high-strength steel (AHSS), follow OEM heat input guidance carefully — excessive heat destroys the engineered strength of these materials.
Squeeze-type resistance spot welding (STRSW) replicates factory spot welds most closely and is the preferred method when the OEM procedure specifies it and panel access allows. Set the machine's pressure, current, and weld time to match the combined metal thickness per the machine manufacturer and I-CAR guidelines.
Welding PPE is non-negotiable: auto-darkening welding helmet (appropriate shade for the process), leather welding gloves, flame-resistant jacket or sleeves, and safety glasses under the helmet. Remove or cover flammable materials in the work area. Keep a fire extinguisher within reach. Follow the shop's lockout/tagout procedures when setting up or servicing welding equipment.
After welding, verify that gaps and flushness meet OEM body specifications before the supervisor approves the repair. Use a tram gauge for diagonal measurements across the opening, or an electronic measuring system if the shop has one. Both diagonal measurements should be equal within the OEM tolerance. Check door, deck lid, or hood gaps with a gap gauge or ruler for uniform spacing. Record your final measurements in the field log next to the RO number.
Your supervisor rates each completed task as Needs Assistance, Meets Standard, or Exceeds Standard on the employer skills checklist. You must receive Meets Standard or better on at least 80 percent of rated tasks in this externship phase to remain on track for a passing employer evaluation. If you receive a Needs Assistance rating, ask your supervisor for specific feedback the same day and request a re-evaluation opportunity on the next appropriate vehicle.
Answer each question, then check it. Nothing is recorded; this is your own practice.
A free tech program — complimentary, as our commitment to get America working. Help us build VoTechWorks. Tell us what works, what doesn’t, and what you want to learn.
Does the school offer financial aid?
No. We don’t offer financial aid because we’re free. No, really: completely free.
Do you offer industry certification?
No. We are not certified yet, so we can’t offer that to students. What we do offer is knowledge and understanding of a trade.
Enroll first in the trade you’re interested in. You get your key, your program opens, and you begin studying.
Enroll free →